This article is a comprehensive collection of tables listing: dangerous reactions of chemicals and designations of etchants; chemical-polishing solutions for irons and steels and nonferrous materials; attack-polishing solutions, macrostructure etchants for iron and steel; and major microstructure etchants for common phases and constituents in ferrous materials.

You do not currently have access to this chapter.
Don't already have an account? Register

Tables of Chemicals and Etchants, Metallography and Microstructures, Vol 9, ASM Handbook, Edited By George F. Vander Voort, ASM International, 2004, p 1094–1114, https://doi.org/10.31399/asm.hb.v09.a0003764