Abstract

This article provides a table that lists the magnetic phase transition temperatures of various chemical elements.

You do not currently have access to this chapter.
Don't already have an account? Register

2016. "Magnetic Phase Transition Temperatures of the Elements", Alloy Phase Diagrams, H. Okamoto, M.E. Schlesinger, E.M. Mueller