Abstract

This article presents ternary alloy phase diagrams to be used primarily by engineers to solve industrial problems. The diagrams presented are for stable equilibrium conditions, with the exception of metastable conditions for some diagrams involving carbon and iron. In some ternary diagrams involving carbon and iron, the symbol M is used to represent both iron and the other metallic element when the two metals substitute for each other in a carbide phase.