This article begins with the one-component, or unary, diagram for magnesium. The diagram shows what phases are present as a function of the temperature and pressure. When two metals are mixed in the liquid state to produce a solution, the resulting alloy is called a binary alloy. The article describes the various types of solid solutions such as interstitial solid solutions and substitutional solid solutions. Free energy is important because it determines whether or not a phase transformation is thermodynamically possible. The article discusses the thermodynamics of phase transformations and free energy, as well as kinetics of phase transformations. It concludes with a description of solid-state phase transformations that occur when one or more parent phases, usually on cooling, produces a phase or phases.

You do not currently have access to this chapter.
Don't already have an account? Register

2016. "Solid Solutions and Phase Transformations", Alloy Phase Diagrams, H. Okamoto, M.E. Schlesinger, E.M. Mueller

Download citation file:


Close
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal