Abstract
This article provides a table that lists the magnetic phase transition temperatures of various chemical elements.
You do not currently have access to this chapter.
Sign in
Don't already have an account? Register
You could not be signed in. Please check your email address / username and password and try again.
ASM members
Member Sign InCitation
Magnetic Phase Transition Temperatures of the Elements, Alloy Phase Diagrams, Vol 3, ASM Handbook, Edited By H. Okamoto, M.E. Schlesinger, E.M. Mueller, ASM International, 2016, p 767–768, https://doi.org/10.31399/asm.hb.v03.a0006248
Download citation file:
ASM INTERNATIONAL
FALL / WINTER 2020 CATALOG
View the new, upcoming, and best-selling resources in ASM Handbooks, technical books, and databases in the Fall / Winter 2020 Catalog.
Related Topics
Related Book Content
The Periodic Table of the Elements
Steel Metallurgy for the Non-Metallurgist
Periodic Table of Elements
Fundamentals of Modeling for Metals Processing
The Chemical Elements
Metals Handbook Desk Edition, 2nd Ed. (2nd Edition)
Periodic Table of Elements
Corrosion: Materials