Abstract

This article is a compilation of ternary alloy phase diagrams for which niobium (Nb) is the first-named element in the ternary system. The diagrams are presented with element compositions in weight percent. The article includes 2 phase diagrams: Nb-Ti-W isothermal section at 600 °C; and Nb-Ti-W isothermal section at 1000 °C.