Abstract

The electrical discharge machining (EDM) process is used for machining dies because of its ability to machining difficult geometries or materials with poor machinability. This article provides a discussion on the fundamentals of electrical discharge erosion and the principles of EDM and orbital-movement EDM. It discusses various aspects of wire EDM in machining dies and provides an overview of the materials used in EDM electrodes. The article concludes with a discussion on electrochemical machining.