This article begins with a discussion on the fundamentals of cutting. It focuses on blanking and piercing operations in a press tool to form and shape the final part geometry. The types of piercing operations include conventional piercing, piercing with a pointed punch, piece-and-extrude operations, slotting, countersinking, and cutting and lancing of tabs. The article provides information on the punch assembly, the die assembly, and the stripper and discusses the factors considered during piercing operations. It reviews the applications of the four types of blanks used in sheet-forming operations, namely, rectangular blank, rough blank, partially developed blank, and fully developed blank. It concludes with a discussion on the process capabilities, applications, and limitations of fine-edge blanking and piercing.

You do not currently have access to this chapter.
Don't already have an account? Register

Blanking and Piercing, Metalworking: Sheet Forming, Vol 14B, ASM Handbook, Edited By S.L. Semiatin, ASM International, 2006, p 130–143, https://doi.org/10.31399/asm.hb.v14b.a0005117

Download citation file:


Close
Close Modal

or Create an Account

Close Modal
Close Modal