Forming of Refractory Metals
-
Published:2006
Abstract
This article describes the formability and surface contamination of the refractory metals such as niobium, tantalum, molybdenum, tungsten, and titanium-zirconium-molybdenum alloys. It reviews the factors that affect mechanical properties and formability during rolling and heat treatment. The effect of temperature on the formability of refractory metals is discussed. The article provides a description of the forming methods of sheet and preformed blanks using refractory metals. It also discusses the types of lubricants, including oils, soaps, waxes, silicones, graphite, and molybdenum disulphide, used in the forming of refractory metals.
Sign in
ASM members
Member Sign InLouis E. Huber, Jr., Christopher A. Michaluk, Forming of Refractory Metals, Metalworking: Sheet Forming, Vol 14B, ASM Handbook, Edited By S.L. Semiatin, ASM International, 2006, p 652–655, https://doi.org/10.31399/asm.hb.v14b.a0005167
Download citation file:
Close
ASM INTERNATIONAL
FALL / WINTER 2020 CATALOG
View the new, upcoming, and best-selling resources in ASM Handbooks, technical books, and databases in the Fall / Winter 2020 Catalog.