Superplastic Sheet Forming
-
Published:2006
Abstract
This article discusses many of the processes and related considerations involved in the forming of superplastic sheet metal parts. It reviews the requirements for superplasticity and describes the characteristics of superplastic metals. The characterization of superplastic behavior includes the characterization of plastic flow, internal cavitation, and fracture behavior. Processing variables needed for the overall characterization of superplastic behavior are summarized. The article discusses the superplastic forming methods, namely, blow forming, vacuum forming, thermoforming, deep drawing, superplastic forming/diffusion bonding, forging, extrusion, and dieless drawing. It provides information on superelastic forming equipment and tooling. The article explains the thinning characteristics and quick plastic forming and its technological elements. It describes the manufacturing practice of the process. The article concludes with a discussion on the superplastic behavior in iron-base alloys.
Sign in
ASM members
Member Sign InA.K. Ghosh, C.H. Hamilton, Superplastic Sheet Forming, Metalworking: Sheet Forming, Vol 14B, ASM Handbook, Edited By S.L. Semiatin, ASM International, 2006, p 345–366, https://doi.org/10.31399/asm.hb.v14b.a0005147
Download citation file:
Close
ASM INTERNATIONAL
FALL / WINTER 2020 CATALOG
View the new, upcoming, and best-selling resources in ASM Handbooks, technical books, and databases in the Fall / Winter 2020 Catalog.