Flanging is a process used to form a projecting rim or edge on a part. This article explores how to determine aluminum flanging limits in terms of fracture, wrinkling, and springback, and their influencing material and process parameters with examples.
You do not currently have access to this chapter.
Sign in
Don't already have an account? Register
You could not be signed in. Please check your email address / username and password and try again.
ASM members
Member Sign InCitation
Jian Cao, Flanging of Aluminum, Metalworking: Sheet Forming, Vol 14B, ASM Handbook, Edited By S.L. Semiatin, ASM International, 2006, p 600–604, https://doi.org/10.31399/asm.hb.v14b.a0005166
Download citation file:
Close
ASM INTERNATIONAL
FALL / WINTER 2020 CATALOG
View the new, upcoming, and best-selling resources in ASM Handbooks, technical books, and databases in the Fall / Winter 2020 Catalog.
Related Topics
Related Book Content
Forming of Advanced High-Strength Steels (AHSS)
Sheet Metal Forming Processes and Applications
Bending of Sheet Metal
Metalworking: Sheet Forming
Design for Sheet Forming
Metalworking: Sheet Forming
Classification and Description of Sheet Metal Forming Operations
Sheet Metal Forming Fundamentals
Green Sand Molding
Casting
Springback
Metalworking: Sheet Forming
Forming of Advanced High-Strength Steels
Metalworking: Sheet Forming
Modeling and Simulation of the Forming of Aluminum Sheet Alloys
Metalworking: Sheet Forming
Bulk Properties of Powders
Powder Metallurgy
Process Simulation
Sheet Metal Forming Processes and Applications