Metalworking: Sheet Forming
Abstract
This article discusses the most important factors required for cutoff methods. It explains the operations of machines used for the punching, shearing, notching, or coping of plates, bars, and structural sections. The article describes the effects of the blade angle and speed on the shear blade life. It reviews the design requirements and best practices for the production of blades. The article compares double-cut dies with single-cut dies used for shearing of structural and bar shapes. The shearing of specific forms, such as angle iron and flat stock, is also discussed. The article describes the advantages of hydraulic bar and structural shears. It concludes with information on the principle and construction of impact cutoff machines.
Sign in
ASM members
Member Sign InShearing of Bars and Bar Sections, Metalworking: Sheet Forming, Vol 14B, ASM Handbook, Edited By S.L. Semiatin, ASM International, 2006, p 445–455, https://doi.org/10.31399/asm.hb.v14b.a0005178
Download citation file:
ASM INTERNATIONAL
FALL / WINTER 2020 CATALOG
View the new, upcoming, and best-selling resources in ASM Handbooks, technical books, and databases in the Fall / Winter 2020 Catalog.