Indirect Nondestructive Measurements of Die Wear in Stamping Productions[1]
-
Published:2006
Abstract
The measurement techniques for die wear can be classified into the following two categories: direct measurements, which are done using lab techniques; and indirect nondestructive measurements, which are done by plant monitoring. This article describes the details of the plant monitoring techniques, along with comprehensive discussions on the measured wear data based on roughness and hardness of die surfaces. It presents a comparison between the predicted and measured die wear rates.
Sign in
ASM members
Member Sign InHuimin Liu, Sriram Sadagopan, Indirect Nondestructive Measurements of Die Wear in Stamping Productions, Metalworking: Sheet Forming, Vol 14B, ASM Handbook, Edited By S.L. Semiatin, ASM International, 2006, https://doi.org/10.31399/asm.hb.v14b.a0009001
Download citation file:
Close
ASM INTERNATIONAL
FALL / WINTER 2020 CATALOG
View the new, upcoming, and best-selling resources in ASM Handbooks, technical books, and databases in the Fall / Winter 2020 Catalog.