Rapid prototyping (RP) techniques in the sheet-metal forming industry is developed to quickly test the form and fit of new sheet-metal products on a prototype basis as well as for production runs characterized by small lot sizes. This article provides an overview of some of the technologies used for RP and low-volume production of sheet-metal parts. It discusses low-cost tooling and flexible sheet-forming processes and reviews the various aspects of incremental sheet forming.

You do not currently have access to this chapter.
Don't already have an account? Register

Lotta Lamminen Vihtonen, Boel Wadman, Torgeir Svinning, Rein Küttner, Rapid Prototyping for Sheet-Metal Forming, Metalworking: Sheet Forming, Vol 14B, ASM Handbook, Edited By S.L. Semiatin, ASM International, 2006, p 851–858, https://doi.org/10.31399/asm.hb.v14b.a0005154