The use of an effective control design, along with high-performance hardware and software for controller implementation, allows the use of feedback process control for manufacturing processes to improve part quality and consistency. This article provides an overview of control system design and its application to various manufacturing processes. It presents various examples of control system applications to show that appropriate control strategies increase the robustness of the processes by eliminating process sensitivity to system variations and external disturbances.

You do not currently have access to this chapter.
Don't already have an account? Register

Mahmoud Y. Demeri, Jian Cao, Ravi Venugopal, Process and Feedback Control for Manufacturing, Metalworking: Sheet Forming, Vol 14B, ASM Handbook, Edited By S.L. Semiatin, ASM International, 2006, p 840–850, https://doi.org/10.31399/asm.hb.v14b.a0005153

Download citation file:


Close
Close Modal

or Create an Account

Close Modal
Close Modal