Abstract

This article begins with a discussion on the factors considered in the selection of bending methods. It presents a detailed description of the types of bending method, machines and tools used in the bending and forming of tubing. The article provides an overview of bending tubing with and without a mandrel and hot bending. It concludes with a discussion on the bending of thin-wall tubes and lubrication for tube bending.