Metalworking: Sheet Forming
Troubleshooting Formability Problems Using Strain Analysis
-
Published:2006
Abstract
This article describes strain analysis techniques for troubleshooting formability and process discrepancies throughout a tooling development and production stamping cycle. The techniques include strain calculations of a flat blank, forming limit curve, and forming limit diagram. The article describes the types of strain analysis, namely, thinning strain analysis and circle grid strain analysis. It also provides information on the applications of the thinning strain analysis.
Sign in
ASM members
Member Sign InDaniel J. Schaeffler, Evan J. Vineberg, Troubleshooting Formability Problems Using Strain Analysis, Metalworking: Sheet Forming, Vol 14B, ASM Handbook, Edited By S.L. Semiatin, ASM International, 2006, p 697–706, https://doi.org/10.31399/asm.hb.v14b.a0005182
Download citation file:
Close
ASM INTERNATIONAL
FALL / WINTER 2020 CATALOG
View the new, upcoming, and best-selling resources in ASM Handbooks, technical books, and databases in the Fall / Winter 2020 Catalog.