This article reviews general trends in the cyclic response for representative commercial alloys to establish the spectrum of cyclic properties attainable through microstructural alteration. Individual alloy classes are examined in detail to assess the understanding of relationships between microstructure and fatigue resistance. These alloys classes include ferritic-pearlitic alloys, martensitic alloys, maraging steels, and metastable austenitic alloys. The article also discusses the role of internal defects and selective surface processing in influencing fatigue performance.

You do not currently have access to this chapter.
Don't already have an account? Register

Ronald W. Landgraf, 1996. "Fatigue Resistance and Microstructure of Ferrous Alloys", Fatigue and Fracture