This article discusses two major approaches in estimating fatigue life from the viewpoint of their use as engineering methods. These include the stress-based (S-N curve) approach and strain-based approach. The stress-based and strain-based approaches are compared, with some comments on their manner of use and limitations. The use of the Palmgren-Miner rule for life prediction for variable amplitude loading is also discussed.