Skip to Main Content

Abstract

This article describes the test methods of fracture toughness, namely, linear-elastic and nonlinear fracture toughness testing methods. Linear-elastic fracture toughness testing includes slow and rapid loading, crack initiation, and crack arrest method. Nonlinear testing comprises JIC testing, J-R curve evaluation, and crack tip opening displacement (CTOD) method. Other methods used include the combined J standard method, the common fracture toughness test, transition fracture toughness testing, and the weldment fracture testing method.