Contact fatigue is a surface-pitting-type failure commonly found in ball or roller bearings. This article discusses the mechanisms of contact fatigue found in gears, cams, valves, rails, and gear couplings. It discusses the statistical analysis of rolling contact bearing-life tests. The article concludes with information on various approaches that improve the contact fatigue resistance of rolling contact systems.

You do not currently have access to this chapter.
Don't already have an account? Register

W.A. Glaeser, S.J. Shaffer, 1996. "Contact Fatigue", Fatigue and Fracture