There are two parts to deal with uncertainty in fatigue design: determining the distributions of possible values for all uncertain inputs and calculating the probability of failure due to all the uncertain inputs. This article discusses the sources of uncertainty in a fatigue analysis, such as the material properties, distribution of applied stress levels within a given environment, environments or loading intensities, and modeling or prediction. It presents a probabilistic approach for analyzing the uncertainties and determining the level of reliability (probability of failure).