This article provides ASTM standard definitions for fatigue and describes the approaches that are used to design finite or infinite life, used in a complementary sense in fatigue design. It explains four distinct phases of fatigue: nucleation, structurally dependent crack propagation, crack propagation, and final instability. The article discusses the significant role that fatigue plays in industrial design applications.