Abstract

This article reviews the influence of local strains and corrosion fatigue on the initiation of fatigue cracks in duplex stainless steels. It provides useful information on fatigue crack growth, fatigue strength, and fracture toughness of duplex stainless steels. The article discusses the fatigue and fracture behavior of duplex stainless steels during stress-corrosion cracking. It details the elevated-temperature properties of duplex stainless steels, such as creep-fatigue behavior and thermal cycling properties.