Wrought powder metallurgy (P/M) high-speed tool steels exhibit better machinability, dimensional control and safety in heat treatment, grindability, and edge toughness during cutting. This article discusses the two stages of machining of P/M tool steels: rough machining, in annealed condition, and finish machining, in hardened-and-tempered condition. It tabulates the composition of commercial crucible particle metallurgy and anti-segregation process tool steels and their typical machining conditions.

You do not currently have access to this chapter.
Don't already have an account? Register

Kenneth E. Pinnow, Carl J. Dorsch, 1989. "Machining of P/M Tool Steels", Machining