This article describes the applications, process capabilities, and limitations and advantages of electrostream and capillary drilling. It describes equipment and tooling used for electrostream and capillary drilling. These include electrostream and capillary drilling machines, power supplies, electrolyte system, part holding fixtures, cathode holders, and cathode tubes. Key process parameters for electrostream and capillary drilling are also discussed.