Abstract
This article discusses various machining techniques of zinc alloy die castings. These include turning, boring, drilling, reaming, tapping, die threading, milling, and sawing. In addition, the article describes the factors that influence machinability of the zinc alloy die castings.
You do not currently have access to this chapter.
Sign in
Don't already have an account? Register
You could not be signed in. Please check your email address / username and password and try again.
ASM members
Member Sign InCitation
Gary Adams, Machining of Zinc Alloy Die Castings, Machining, Vol 16, ASM Handbook, ASM International, 1989, p 831–834, https://doi.org/10.31399/asm.hb.v16.a0002187
Download citation file:
Close
ASM INTERNATIONAL
FALL / WINTER 2020 CATALOG
View the new, upcoming, and best-selling resources in ASM Handbooks, technical books, and databases in the Fall / Winter 2020 Catalog.
Related Topics
Related Book Content
Machining of Refractory Metals
Machining
Machining of Tool Steels
Machining
Machining of Powder Metallurgy Materials
Machining
Machining of Cast Irons
Machining
Machining of Nickel and Nickel Alloys
Machining
Machining of Reactive Metals
Machining
Machining of Heat-Resistant Alloys
Machining
Machining of Stainless Steels
Machining