Book Chapter
Trepanning
-
Published:1989
Abstract
Trepanning is used in at least four distinct production applications: round disks, large shallow through holes, circular grooves, and deep holes. This article provides an overview of the first three applications. It describes the machines, tools, techniques, and cutting fluids used for deep-hole trepanning. The article contains a table that lists speeds and feeds for the deep-hole trepanning of various steels with high-speed tool steels and carbide tools.
You do not currently have access to this chapter.
Sign in
Don't already have an account? Register
You could not be signed in. Please check your email address / username and password and try again.
ASM members
Member Sign InCitation
Trepanning, Machining, Vol 16, ASM Handbook, ASM International, 1989, p 175–180, https://doi.org/10.31399/asm.hb.v16.a0002131
Download citation file:
Close
ASM INTERNATIONAL
FALL / WINTER 2020 CATALOG
View the new, upcoming, and best-selling resources in ASM Handbooks, technical books, and databases in the Fall / Winter 2020 Catalog.
Related Book Content
Laser Beam Machining
Machining
Machining of Refractory Metals
Machining
Shaping and Slotting
Machining
Machining of Cast Irons
Machining
Surface Engineering of Carbide, Cermet, and Ceramic Cutting Tools
Surface Engineering
High-Speed Tool Steels
Machining
P/M High-Speed Tool Steels
Machining
Heat Treating of Tool Steels
Metals Handbook Desk Edition, 2nd Ed. (2nd Edition)
Wrought Tool Steels
Properties and Selection: Irons, Steels, and High-Performance Alloys