Machining
Machining of Tool Steels
-
Published:1989
Abstract
This article describes the selection of tool steels on the basis of specific product applications. It contains tables that list nominal speeds and feeds for the machining of various tool steels. The machining processes include turning, boring, broaching, drilling, reaming, tapping, milling, and sawing. The article explains the machining of the following tool steels: water hardening; types A, D and O cold-work; hot work; high speed, low-alloy special-purpose; and low-carbon mold. It details the machining of tool steel gears. The article also discusses the grinding of tool steels based on steel classification and the effects of steel composition and hardness on grindability. It reviews the types of grinding, namely, surface grinding, cylindrical grinding, centerless grinding, internal grinding, thread grinding, flute grinding, and low-stress grinding. Grinding of types-A, D, F, L, O, P, S and W steels, hot-work steels, and high speed steels, is also detailed.
Sign in
ASM members
Member Sign InMachining of Tool Steels, Machining, Vol 16, ASM Handbook, ASM International, 1989, p 708–732, https://doi.org/10.31399/asm.hb.v16.a0002181
Download citation file:
ASM INTERNATIONAL
FALL / WINTER 2020 CATALOG
View the new, upcoming, and best-selling resources in ASM Handbooks, technical books, and databases in the Fall / Winter 2020 Catalog.