Machining
Abstract
This article discusses the manufacturing steps and compositions of cemented carbides, as well as their microstructure, classifications, applications, and physical and mechanical properties. It provides information on new tool geometries, tailored substrates, and the application of thin and hard coatings to cemented carbides by chemical vapor deposition and physical vapor deposition. The article also discusses tool wear mechanisms and the methods available for holding the carbide tool.
Sign in
ASM members
Member Sign InA.T. Santhanam, P. Tierney, Cemented Carbides, Machining, Vol 16, ASM Handbook, ASM International, 1989, p 71–89, https://doi.org/10.31399/asm.hb.v16.a0002124