Abstract
This article focuses on the machining of reactive metals which refer collectively to the elements titanium, hafnium, and zirconium. It provides guidelines for machining titanium and titanium alloys and describes machining operations, such as turning, milling, drilling, tapping, reaming, grinding, and sawing, performed on titanium and its alloys. The article also provides information on electrochemical machining (ECM), chemical milling (CHM), and laser beam machining (LBM) for titanium and titanium alloys. Guidelines for machining zirconium alloys and hafnium are also provided. The article provides a short description of turning, milling, and drilling operations performed on zirconium alloys and hafnium. It also discusses health and safety considerations related to zirconium and hafnium.
Sign in
ASM members
Member Sign InHarry E. Chandler, Machining of Reactive Metals, Machining, Vol 16, ASM Handbook, ASM International, 1989, p 844–857, https://doi.org/10.31399/asm.hb.v16.a0002189
Download citation file:
ASM INTERNATIONAL
FALL / WINTER 2020 CATALOG
View the new, upcoming, and best-selling resources in ASM Handbooks, technical books, and databases in the Fall / Winter 2020 Catalog.