Planing is a machining process for removing metal from surfaces in horizontal, vertical, or angular planes. This article discusses the process capabilities of planing and the operations of double-housing and open-side planers. It reviews workpiece setup procedures, including platelike workpieces, irregularly shaped workpieces, and workpieces used for tandem planning. The article provides information on the applications of high-speed steels and carbides in planer tools. It analyzes the tools available in a variety of configurations suited to the undercutting, slotting, and straight planing of either horizontal or vertical surfaces. These include carbide roughing, finishing, gooseneck-holder finishing, and double-cutting tools. The article lists recommended speeds and feeds for planing with high-speed steel or carbide tools. It concludes with a comparison of planing with sawing and milling.

You do not currently have access to this chapter.
Don't already have an account? Register
Close Modal

or Create an Account

Close Modal
Close Modal