ASM Handbook
Machining
ASM International
Volume
16
ISBN electronic:
978-1-62708-188-7
Publication date:
1989
Abstract
This article provides an overview of the independent and dependent variables of a machining process. Independent variables include workpiece material, specific machining processes, and tool materials and geometry. Cutting force and power, surface finish, and tool wear and failure are some dependent variables discussed. The article also describes the relations between the input variables and process behavior.
You do not currently have access to this chapter.
Sign in
Don't already have an account? Register
You could not be signed in. Please check your email address / username and password and try again.
ASM members
Member Sign InCitation
J. T. Black, 1989. "Introduction to Machining Processes", Machining
Download citation file:
Close
ASM Reference Publications Catalog
The new Fall / Winter 2019-2020 Catalog features more than 200 new and upcoming releases and our popular best-selling titles. Save now with prepublication pricing and set sales.