Volume 16 covers machining technologies, including fundamentals, detailed descriptions of specific machining and grinding processes, guidelines for proper selection of cutting tool materials and cutting fluids, and recommendations for improved machining productivity and efficiency. The volume, featuring 1,300 illustrations and 620 tables, includes process capabilities, machines, cutting parameters plus variables, and applications of traditional machining processes such as turning, drilling, and milling. Mechanical, electrical, thermal, and chemical material removal procedures are also summarized. For information on the print version of Volume 16, ISBN 978-0-87170-022-3, follow this link.
Machining
DOI: https://doi.org/10.31399/asm.hb.v16.9781627081887
ISBN (electronic): 978-1-62708-188-7
Publisher: ASM International
Published: 1989
Download citation file:
Close
Table of Contents
-
Introduction to Machining Processes
-
Fundamentals of the Machining Process
-
Forces, Power, and Stresses in MachiningByPaul H. CohenPaul H. CohenThe Pennsylvania State UniversitySearch for other works by this author on:
-
Surface Finish and Surface IntegrityByMichael Field;Michael FieldMetcut Research Associates Inc.Search for other works by this author on:John F. Kahles;John F. KahlesMetcut Research Associates Inc.Search for other works by this author on:William P. KosterWilliam P. KosterMetcut Research Associates Inc.Search for other works by this author on:
-
Tool Wear and Tool LifeByL. Alden KendallL. Alden KendallWashington State UniversitySearch for other works by this author on:
-
Cutting Tool Materials
-
P/M High-Speed Tool SteelsByKenneth E. Pinnow;Kenneth E. PinnowRevising authorCrucible Materials CorporationSearch for other works by this author on:William StaskoWilliam StaskoRevising authorCrucible Materials CorporationSearch for other works by this author on:
-
CermetsByWalter W. GrussWalter W. GrussKyocera Feldmuehle, Inc.Search for other works by this author on:
-
CeramicsByRanga Komanduri;Ranga KomanduriNational Science FoundationSearch for other works by this author on:Shyam K. SamantaShyam K. SamantaNational Science FoundationSearch for other works by this author on:
-
Ultrahard Tool MaterialsByP.J. HeathP.J. HeathDe Beers Industrial Diamond Division (Pty) Ltd.(England)Search for other works by this author on:
-
Cutting Fluids
-
Metal Cutting and Grinding FluidsByElliot S. NachtmanElliot S. NachtmanTower Oil & Technology CompanySearch for other works by this author on:
-
-
Traditional Machining Processes
-
TappingByMark JohnsonMark JohnsonRevising authorTapmatic CorporationSearch for other works by this author on:
-
Gear ManufactureByTheodore J. Krenzer;Theodore J. KrenzerRevising authorThe Gleason Works, Division of Gleason CorporationSearch for other works by this author on:Joseph W. ConiglioJoseph W. ConiglioRevising authorGould & Eberhardt Gear Machinery CorporationSearch for other works by this author on:
-
SawingByTed A. SlezakTed A. SlezakRevising authorArmstrong-Blum Manufacturing CompanySearch for other works by this author on:
-
Proper FixturingByClifford E. DrakeClifford E. DrakeENERPAC Group Applied Power, Inc.Search for other works by this author on:
-
Grinding, Honing, and Lapping
-
Principles of GrindingByRichard P. LindsayRichard P. LindsayNorton CompanySearch for other works by this author on:
-
LappingByPel LynahPel LynahRevising authorP.R. Hoffman Machine ProductsSearch for other works by this author on:
-
-
Nontraditional Machining Processes
-
Introduction to Nontraditional Machining ProcessesByGary F. BenedictGary F. BenedictAllied-Signal Aerospace Company, Garrett Engine DivisionSearch for other works by this author on:
-
Abrasive Jet MachiningByGlenn E. StorckGlenn E. StorckS.S. White Industrial Products, Division of Pennwalt CorporationSearch for other works by this author on:
-
Abrasive Flow MachiningByLawrence J. Rhoades;Lawrence J. RhoadesExtrude Hone CorporationSearch for other works by this author on:Hilary A. ClouserHilary A. ClouserExtrude Hone CorporationSearch for other works by this author on:
-
Ultrasonic MachiningByWilliam R. TyrrellWilliam R. TyrrellBranson Ultrasonics CorporationSearch for other works by this author on:
-
Electrochemical MachiningByTerry L. LievestroTerry L. LievestroRevising authorLehr Precision, Inc.Search for other works by this author on:
-
Electrochemical GrindingByRobert E. PhillipsRobert E. PhillipsEverite Machine Products CompanySearch for other works by this author on:
-
Electrical Discharge MachiningByJohn E. FullerJohn E. FullerRockwell InternationalSearch for other works by this author on:
-
Electron Beam MachiningByRonald W. SchneiderRonald W. SchneiderMG Industries, Systems DivisionSearch for other works by this author on:
-
Thermal Energy MethodByThomas FisherThomas FisherSurftran, Division of Robert Bosch CorporationSearch for other works by this author on:
-
Chemical MillingByEugene M. LangworthyEugene M. LangworthyAerochem, Inc.Search for other works by this author on:
-
Photochemical MachiningByHoward FriedmanHoward FriedmanFotofabrication CorporationSearch for other works by this author on:
-
-
High-Productivity Machining
-
Machine Controls and Computer Applications in Machining
-
Numerical ControlByYoram KorenYoram KorenThe University of MichiganSearch for other works by this author on:
-
Adaptive ControlByA. Galip UlsoyA. Galip UlsoyUniversity of MichiganSearch for other works by this author on:
-
CAD/CAM Applications in MachiningByEmory W. Zimmers, Jr.Emory W. Zimmers, Jr.Lehigh UniversitySearch for other works by this author on:
-
-
Machining of Specific Metals and Alloys
-
Machining of Carbon and Alloy SteelsByM.E. FinnM.E. FinnSteltech, a subsidiary of Stelco, Inc.Search for other works by this author on:
-
Machining of Stainless SteelsByRonald P. Ney, Sr.Ronald P. Ney, Sr.Carpenter Technology CorporationSearch for other works by this author on:
-
Machining of P/M Tool SteelsByKenneth E. Pinnow;Kenneth E. PinnowCrucible Materials CorporationSearch for other works by this author on:Carl J. DorschCarl J. DorschCrucible Materials CorporationSearch for other works by this author on:
-
Machining of Nickel and Nickel AlloysByR.W. BreitzigR.W. BreitzigRevising authorINCO Alloys InternationalSearch for other works by this author on:
-
Machining of Reactive MetalsByHarry E. ChandlerHarry E. ChandlerASM InternationalSearch for other works by this author on:
-
Machining of Refractory MetalsByHarry E. ChandlerHarry E. ChandlerASM InternationalSearch for other works by this author on:
-
Machining of Beryllium[1]ByDouglas V. Gallagher;Douglas V. GallagherRockwell InternationalSearch for other works by this author on:R.E. HardestyR.E. HardestyElectrofusion CorporationSearch for other works by this author on:
-
Machining of Uranium and Uranium AlloysByJames A. ArisJames A. ArisRockwell InternationalSearch for other works by this author on:
-
Machining of Powder Metallurgy MaterialsByHarry E. ChandlerHarry E. ChandlerASM InternationalSearch for other works by this author on:
-
Machining of Metal-Matrix Composites and Honeycomb StructuresByHarry E. ChandlerHarry E. ChandlerASM InternationalSearch for other works by this author on:
-