Hot Working Simulation by Hot Torsion Testing[1]

By
Joseph R. Pickens
Joseph R. Pickens
Concurrent Technologies Corporation
Search for other works by this author on:
Published:
2005
Publication history
March 09, 2009

Abstract

This article summarizes the types of hot working simulation tests such as hot tension, compression, and torsion testing used in the assessment of workability. It illustrates the use of hot torsion testing for the optimization of hot working processes. The article concludes with information on some hot torsion application examples.

You do not currently have access to this content.
Don't already have an account? Register

Joseph R. Pickens, 2005. "Hot Working Simulation by Hot Torsion Testing", Metalworking: Bulk Forming, S.L. Semiatin