In terms of the design of a forging, flash is an excess or surplus of metal that is trimmed or otherwise removed after forging operations are completed. This article discusses flash components and the functions of flash. It describes a series of conventional and unconventional flash designs and design adjustments, covering several forging processes and configurations. The article concludes with information on the checklists for the convenience of both designers of forgings and designers of forging dies and contiguous flash.