Abstract

Radial forging is a hot- or cold-forming process that uses two or more radially moving anvils or dies to produce solid or tubular components with constant or varying cross sections along their lengths. This article focuses on the workpiece configuration, workpiece materials, machines, dies, advantages, and limitations of radial forging. It concludes with a discussion on the applications of radial forging.