Abstract

A wide range of flow-formed open- and close-ended shapes are currently available in a variety of difficult-to-form materials, including titanium alloys and nickel-base super alloys. This article describes the two basic methods of flow forming that are characterized by the position of the rolls during the forming process. The flow forming methods include staggered-roll flow forming process and in-line flow-forming process. Typical mechanical properties of flow-formed materials in various conditions are summarized in a table. Proper process controls and subsequent product qualification tests are critical to assure optimal performance of the flow-formed tubular component. The article discusses the most commonly required process control parameters and the effects of forming speed and temperature in the flow forming process.

You do not currently have access to this chapter.
Don't already have an account? Register

George Ray, Deniz Yilmaz, Matthew Fonte, Richard P. Keele, 2005. "Flow Forming", Metalworking: Bulk Forming, S.L. Semiatin

Download citation file:


Close
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal