Thermomechanical are used to gain insight into the causes of problems that arise during a given thermomechanical process. This article provides examples to demonstrate how significant the parameters were selected for specific tests. It examines the types of problems that can occur during a thermomechanical process. The article provides information on the thermophysical properties, which include specific heat, coefficient of thermal expansion, thermal conductivity/diffusivity, and density. It concludes with examples that illustrate how the various considerations in testing are successfully used to solve practical thermomechanical processing problems.

You do not currently have access to this chapter.
Don't already have an account? Register

Stéphane Guillard, Koushik Ray, Thermomechanical Testing, Metalworking: Bulk Forming, Vol 14A, ASM Handbook, Edited By S.L. Semiatin, ASM International, 2005, https://doi.org/10.31399/asm.hb.v14a.a0009013

Download citation file:


Close
Close Modal

or Create an Account

Close Modal
Close Modal