Failures of Springs[1]

By
James H. Maker
James H. Maker
Consultant, Associated Spring
Search for other works by this author on:
Published:
2002

Abstract

This article discusses the common causes of failures of springs, with illustrations. Design deficiencies, material defects, processing errors or deficiencies, and unusual operating conditions are the common causes of spring failures. In most cases, these causes result in failure by fatigue. The article describes the operating conditions of springs, common failure mechanisms, and presents an examination of the failures that occur in springs.

You do not currently have access to this content.
Don't already have an account? Register

James H. Maker, 2002. "Failures of Springs", Failure Analysis and Prevention, William T. Becker, Roch J. Shipley