Fatigue Fracture Appearances
-
Published:2002
Abstract
This article commences with a summary of fatigue processes and mechanisms. It focuses on fractography of fatigue. Characteristic fatigue fracture features that can be discerned visually or under low magnification are described. Typical microscopic features observed on structural metals are presented subsequently, followed by a brief discussion of fatigue in nonmetals. The article reviews the various macroscopic and microscopic features to characterize the history and growth rate of fatigue in metals. It concludes with a description of fatigue of polymers and composites.
Sign in
ASM members
Member Sign InRussell A. Lund, Shahram Sheybany, Fatigue Fracture Appearances, Failure Analysis and Prevention, Vol 11, ASM Handbook, Edited By William T. Becker, Roch J. Shipley, ASM International, 2002, p 627–640, https://doi.org/10.31399/asm.hb.v11.a0003539
Download citation file:
Close
ASM INTERNATIONAL
FALL / WINTER 2020 CATALOG
View the new, upcoming, and best-selling resources in ASM Handbooks, technical books, and databases in the Fall / Winter 2020 Catalog.