Failure Analysis and Prevention
Rolling-Contact Fatigue of Ceramics
-
Published:2002
Abstract
Rolling-contact fatigue (RCF) is a surface damage process due to the repeated application of stresses when the surfaces of two bodies roll on each other. This article briefly describes the various surface cracks caused by manufacturing processing faults or blunt impact loads on ceramic balls surfaces. It discusses the propagation of fatigue cracks involved in rolling contacts. The characteristics of various types of RCF test machines are summarized. The article concludes with a discussion on the various failure modes of silicon nitride in rolling contact. These include the spalling fatigue failure, the delamination failure, and the rolling-contact wear.
Sign in
ASM members
Member Sign InY. Wang, M. Hadfield, Rolling-Contact Fatigue of Ceramics, Failure Analysis and Prevention, Vol 11, ASM Handbook, Edited By William T. Becker, Roch J. Shipley, ASM International, 2002, p 957–964, https://doi.org/10.31399/asm.hb.v11.a0003564
Download citation file:
Close
ASM INTERNATIONAL
FALL / WINTER 2020 CATALOG
View the new, upcoming, and best-selling resources in ASM Handbooks, technical books, and databases in the Fall / Winter 2020 Catalog.