This article contains a table that lists the properties of various fuel gases, namely, acetylene, hydrogen, methane, methyl acetylene propadiene, propane, propylene, and natural gas. It discusses shielding gases, their mixtures and uses in gas metal arc welding, flux cored arc welding, gas tungsten arc welding, and plasma arc welding.