This article describes compounds developed to enhance the penetration of the gas tungsten arc welding (GTAW) process. Penetration-enhanced GTAW processes have been referred to variously as Flux TIG, A-TIG, and GTAW with a penetration-enhancing compound (PEC). In all cases, the process uses a material that is not a flux but rather an oxide or mixture of oxides. The productivity of traditional GTAW is limited for many applications because of low deposition rates, shallow penetration (typically 3 mm, or ? in.), or inconsistent penetration. Penetration-enhanced GTAW processes can increases weld penetration by as much as 300% and reduces heat-to-heat variation in penetration and distortion.

You do not currently have access to this chapter.
Don't already have an account? Register

Ian D. Harris, 2011. "Gas Tungsten Arc Welding with Penetration-Enhancing Compounds", Welding Fundamentals and Processes, T. Lienert, T. Siewert, S. Babu, V. Acoff

Download citation file:


Close
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal