Qualification of welding procedures and personnel is an important step to assure the quality and performance of any welded component or structure. This article summarizes common welding procedures, personnel qualification variables, and test methods. Welding procedure qualification tests can be categorized as either standard or special. The article discusses the purpose of qualifying a welding procedure to demonstrate that the resulting welds will meet prescribed quality standards and the qualification of the personnel.

You do not currently have access to this chapter.
Don't already have an account? Register

Harvey R. Castner, 2011. "Qualification of Welding Procedures and Personnel", Welding Fundamentals and Processes, T. Lienert, T. Siewert, S. Babu, V. Acoff