Abstract

This article discusses three distinct mechanisms of bonding for solid-state (forge) welding processes, namely, contaminant displacement/interatomic bonding, dissociation of retained oxides, and decomposition of the interfacial structure. It explains the processes that can be characterized as having two stages: heating and forging. The article also includes a table that illustrates weld strengths as a function of annealing temperature for a range of materials.

You do not currently have access to this chapter.
Don't already have an account? Register

Jerry E. Gould, 2011. "Mechanisms of Bonding for Solid-State Welding Processes", Welding Fundamentals and Processes, T. Lienert, T. Siewert, S. Babu, V. Acoff