Skip to Main Content
ASM Handbook

Welding Fundamentals and Processes

Edited by
T. Lienert
T. Lienert
Search for other works by this author on:
;
T. Siewert
T. Siewert
Search for other works by this author on:
;
S. Babu
S. Babu
Search for other works by this author on:
;
V. Acoff
V. Acoff
Search for other works by this author on:
ASM International
Volume
6A
ISBN electronic:
978-1-62708-174-0
Publication date:
2011
Book Chapter

Numerical Aspects of Modeling Welds[1]

By
John Goldak
John Goldak
Carleton University
Search for other works by this author on:
;
Mahyar Asadi
Mahyar Asadi
Carleton University
Search for other works by this author on:
;
Lennart Karlsson
Lennart Karlsson
LuleƄ University of Technology
Search for other works by this author on:
Published:
2011
Page range:
819 - 829
Publication history
June 20, 2011

Abstract

This article is a comprehensive collection of formulas and numerical solutions, addressing many heat-transfer scenarios encountered in welds. It provides detailed explanations and dimensioned drawings in order to discuss the geometry of weld models, transfer of energy and heat in welds, microstructure evaluation, thermal stress analysis, and fluid flow in the weld pool.

You do not currently have access to this content.
Don't already have an account? Register

John Goldak, Mahyar Asadi, Lennart Karlsson, 2011. "Numerical Aspects of Modeling Welds", Welding Fundamentals and Processes, T. Lienert, T. Siewert, S. Babu, V. Acoff

Download citation file:


Close
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal