This article describes the fundamental aspects of three nondestructive evaluation (NDE) methods of solid-state welds in terms of operation principles. These methods are radiography, ultrasound, and eddy current methods. The article provides examples of these NDE techniques performed on various types of flaws resulting from solid-state welding processes.