Electroslag and Electrogas Welding[1]

By
S.D. Brandi
S.D. Brandi
Revising author
Escola de Politecnica da USP
Search for other works by this author on:
;
S. Liu
S. Liu
Revising author
Colorado School of Mines
Search for other works by this author on:
;
R.D. Thomas, Jr.
R.D. Thomas, Jr.
Revising author
R.D. Thomas and Company
Search for other works by this author on:
Published:
2011
Page range:
365 - 379
Publication history
June 20, 2011

Abstract

Electroslag welding (ESW) involves high energy input relative to other welding processes, resulting generally in inferior mechanical properties and specifically in lower toughness of the heat-affected zone. Electrogas welding (EGW) is a method of gas metal or flux cored arc welding, wherein an external gas is supplied to shield the arc, and molding shoes are used to confine the molten weld metal for vertical-position welding. This article describes the fundamentals, temperature relations, consumables, metallurgical and chemical reactions, and process development of ESW. The problems, quality control, and process applications of ESW and EGW are also discussed.

You do not currently have access to this content.
Don't already have an account? Register

S.D. Brandi, S. Liu, R.D. Thomas, Jr., 2011. "Electroslag and Electrogas Welding", Welding Fundamentals and Processes, T. Lienert, T. Siewert, S. Babu, V. Acoff

Download citation file:


Close
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal