Welding Fundamentals and Processes
Abstract
This article serves as a basic information source for those interested in accomplishing one-sided, no-hole attachment of metal fasteners. The stud arc-welding process is a substitute for fastening procedures such as drilling and tapping, bolting, and self-tapping screws. The article describes the operating principle of, and the tooling and equipment used for, the welding process. It contains tables that present information on the mechanical properties of aluminum, stainless steel, and low-carbon steel stud arc welded fasteners. The article details the different tests conducted to ensure the quality of stud arc-welded fasteners. It concludes with information on safety precautions to be followed in the welding process.
Sign in
ASM members
Member Sign InStud Arc Welding, Welding Fundamentals and Processes, Vol 6A, ASM Handbook, Edited By T. Lienert, T. Siewert, S. Babu, V. Acoff, ASM International, 2011, p 380–390, https://doi.org/10.31399/asm.hb.v06a.a0005555
Download citation file:
Close
ASM INTERNATIONAL
FALL / WINTER 2020 CATALOG
View the new, upcoming, and best-selling resources in ASM Handbooks, technical books, and databases in the Fall / Winter 2020 Catalog.